Mechanical properties
Hardness Shore D
Sh. D
DIN 53 505
62 - 64
Ball pressure hardness
N/mm²
0
Tensile strength (23°C)
N/mm²
DIN 53 455
10 - 14
Elongation at break (23°C)
%
DIN 53 455
100 - 130
Tensile modulus (23°C)
N/mm²
DIN 53 457
0
PV-limit 3 m/min
N.M/mm².min
26
PV-limit 30 m/min
N.M/mm².min
28
PV-limit 300 m/min
N.M/mm².min
29
Coëff. Of friction - statical
0.15
Coefficient of friction v-steel - Dynamic
0
Wear K.10-8
cm³.min/kg.m.h
5.9
Physical properties
Deformation after 24h at 23°C - 15 N/mm²
%
ASTM-D621
4.2
Deformation after 24h at 260°C - 4 N/mm²
%
ASTM-D621
3
Compr. Strength at 1% deformation (23°C)
N/mm²
DIN 53 454
12.5
Electrical properties
Dielectric strength
KV/mm
0
Thermal properties
Coefficient of thermal expansion (20-100°C)
1/K.10-5
0
Coefficient of thermal expansion (20-150°C)
1/K.10-5
9.2
Coefficient of thermal expansion (150-260°C)
1/K.10-5
12.5
Thermal conductivity (23°C)
W/K.m
DIN 52 612
0.85
Maximum Continuous operating temperature
°C
250
Minimum Continuous operating temperature
°C
-200