Mechanical properties
Hardness Shore D
Sh. D
DIN 53 505
63 - 66
Ball pressure hardness
N/mm²
0
Tensile strength (23°C)
N/mm²
DIN 53 455
14 - 18
Elongation at break (23°C)
%
DIN 53 455
120 - 180
Tensile modulus (23°C)
N/mm²
DIN 53 457
1420
PV-limit 3 m/min
N.M/mm².min
35
PV-limit 30 m/min
N.M/mm².min
35
PV-limit 300 m/min
N.M/mm².min
39
Coëff. Of friction - statical
0.15
Coefficient of friction v-steel - Dynamic
0
Wear K.10-8
cm³.min/kg.m.h
5.5
Physical properties
Deformation after 24h at 23°C - 15 N/mm²
%
ASTM-D621
3
Deformation after 24h at 260°C - 4 N/mm²
%
ASTM-D621
1.6
Compr. Strength at 1% deformation (23°C)
N/mm²
DIN 53 454
15
Electrical properties
Dielectric strength
KV/mm
0
Thermal properties
Coefficient of thermal expansion (20-100°C)
1/K.10-5
0
Coefficient of thermal expansion (20-150°C)
1/K.10-5
7
Coefficient of thermal expansion (150-260°C)
1/K.10-5
10
Thermal conductivity (23°C)
W/K.m
DIN 52 612
0.72
Maximum Continuous operating temperature
°C
250
Minimum Continuous operating temperature
°C
-200