Mechanical properties
Hardness Shore D
Sh. D
DIN 53 505
56 - 60
Ball pressure hardness
N/mm²
0
Tensile strength (23°C)
N/mm²
DIN 53 455
20 - 26
Elongation at break (23°C)
%
DIN 53 455
220 - 300
Tensile modulus (23°C)
N/mm²
DIM 53 457
800
PV-limit 3 m/min
N.M/mm².min
--
25
PV-limit 30 m/min
N.M/mm².min
--
29
PV-limit 300 m/min
N.M/mm².min
--
32
Coëff. Of friction - statical
--
0.15
Coefficient of friction v-steel - Dynamic
0
Wear K.10-8
cm³.min/kg.m.h
--
6.4
Physical properties
Deformation after 24h at 23°C - 15 N/mm²
%
ASTM D621
8
Deformation after 24h at 260°C - 4 N/mm²
%
ASTM D621
3.6
Compr. Strength at 1% deformation (23°C)
N/mm²
DIN 53 454
7.8
Electrical properties
Dielectric strength
KV/mm
0
Thermal properties
Coefficient of thermal expansion (20-100°C)
1/K.10-5
0
Coefficient of thermal expansion (20-150°C)
1/K.10-5
--
10
Coefficient of thermal expansion (150-260°C)
1/K.10-5
--
13
Thermal conductivity (23°C)
W/K.m
DIN 52 612
0.46
Maximum Continuous operating temperature
°C
--
250
Minimum Continuous operating temperature
°C
--
-200